CNC Turning for Titanium Grade 5 (Ti-6Al-4V)
Turning titanium Grade 5 requires careful parameter control due to its poor thermal conductivity, high strength, and chemical affinity with tool materials. Rigid setups and sharp tooling are mandatory.
권장 가공 매개변수
| 매개변수 | 값 |
|---|---|
| 달성 가능 공차 | ±0.02 mm (±0.0008") |
| 표면 조도 | Ra 0.8-3.2 μm |
| 절삭 속도 | 40-80 m/min |
| 이송 속도 | 0.10-0.20 mm/rev |
| 공구 추천 | Uncoated carbide (S grade) or PVD coated. Sharp positive inserts. Consider PCD for finishing. |
전문가 가공 팁
1
Low cutting speeds — heat has nowhere to go
2
Maintain positive chip flow at all times
3
High-pressure coolant aimed precisely at cutting zone
4
Use C-style or rhombic inserts for better heat dissipation
5
Never recut chips — they work-harden instantly
일반 가공 부품
Medical implant shafts
Aerospace fasteners
Turbine shaft sleeves
Valve stems
Racing axle components
가공 과제
- Chemical reaction with tool coatings
- Chip can ignite if too thin
- Spring-back causes dimensional issues
- Requires specialized coolant management