303 vs 304 vs 316 Stainless Steel: Which Grade to Specify for Machined Parts

303 vs 304 vs 316 stainless for CNC parts: machinability, corrosion resistance, welding, EN numbers 1.4305/1.4301/1.4401, passivation and drawing notes.

Last updated:

Choose 303 when the part is heavily machined, will not be welded and sees only mild environments; choose 304 as the general-purpose grade when you need better corrosion resistance or welding; choose 316 (or 316L) when the part meets chlorides — salt spray, seawater, de-icing salts, many cleaning chemicals. In EN terms these are 1.4305, 1.4301 and 1.4401 / 1.4404.

All three are austenitic chromium-nickel stainless steels, non-magnetic in the annealed condition and not hardenable by heat treatment. The differences are small on a data sheet but large on the shop floor and in service: 303 cuts much more easily, while 304 and 316 resist corrosion better and weld cleanly. This guide explains the trade-offs and what to write on the drawing so the grade, condition and passivation are not left to assumption.

The three grades side by side

Use the bullets below as a quick reference. EN numbers come from EN 10088; JIS equivalents are SUS303, SUS304 and SUS316. Composition ranges differ slightly between standards, so name the standard you buy to if the part is critical.

  • 303 (1.4305, X8CrNiS18-9): 18 % Cr / 9 % Ni base with a deliberate sulfur addition of roughly 0.15–0.35 %. Free-machining; lowest corrosion resistance and toughness of the three; not recommended for welding.
  • 304 (1.4301, X5CrNi18-10): the standard austenitic grade. Good general corrosion resistance, good weldability, gummy to machine. Low-carbon 304L (1.4307) is preferred for welded parts.
  • 316 (1.4401, X5CrNiMo17-12-2) and 316L (1.4404): about 2–3 % molybdenum added, which improves resistance to pitting and crevice corrosion in chloride environments. Machines similarly to 304, slightly tougher on tools.
  • All three: non-magnetic when annealed, but cold work (and heavy machining on 304) can make the surface slightly magnetic.

Machinability: why 303 exists

Austenitic stainless steels work-harden quickly and form long, stringy chips. On a CNC lathe this means chips wrapping around the part and tool, built-up edge, and a work-hardened skin if the tool rubs instead of cuts. 304 and 316 are machinable with sharp positive-rake tools, steady feeds and good coolant, but cycle times are longer and tool wear is higher than in carbon steel.

In 303 the sulfur forms manganese sulfide inclusions that act as chip breakers. Chips break into short segments, surface finish is easier to achieve and tool life improves. Material suppliers commonly quote a machinability rating for 303 of roughly 75 % of the free-cutting steel reference, well above 304 and 316. For turned parts with lots of features — fittings, connectors, pins, spacers — 303 can reduce machining time noticeably.

  • Avoid interrupting a cut or letting the tool dwell on 304/316; the work-hardened layer makes the next pass harder.
  • Small drilled holes and fine threads in 304/316 are where most cost goes; ask whether a feature can be larger or shorter.
  • Thin-walled 304/316 parts deflect and spring back more than aluminum; allow realistic tolerances on thin walls.

Corrosion: the price of free machining

The same sulfide inclusions that help machining are weak points for corrosion. On a 303 surface they can act as pit initiation sites, especially in chloride or acidic environments, so 303 is generally rated below 304 for corrosion resistance. It is fine for indoor equipment, dry mechanisms and many instrument parts, but a poor choice for marine hardware, food contact surfaces with salty or acidic media, or anything washed with chlorinated cleaners.

316 is the normal step up when chlorides are present. Molybdenum improves pitting and crevice resistance, which matters around fasteners, O-ring grooves and tight joints where stagnant liquid sits. 316 is not immune — warm seawater and strong chloride solutions can still attack it — but it is the usual minimum for outdoor coastal use.

Welding and the L grades

If the machined part will be welded, rule out 303: the sulfur makes it prone to hot cracking. Between 304 and 316, the welding behaviour is similar. Standard-carbon grades can form chromium carbides in the heat-affected zone (sensitization), which lowers local corrosion resistance; the low-carbon L grades (304L, 316L) reduce this risk and are the normal choice for welded assemblies. Many mills supply dual-grade 304/304L and 316/316L bar that meets both specifications.

Passivation: ASTM A967, ASTM A380 and AMS 2700

Machining leaves free iron from tools and fixtures on the surface. Passivation is a chemical treatment, usually nitric or citric acid, that removes free iron and lets the chromium oxide layer re-form evenly. It does not change dimensions and does not change appearance much.

  • ASTM A967 is the passivation specification: it lists nitric, citric and other treatments and the tests used to verify the result. Quote it with the method if you care, e.g. “Passivate per ASTM A967, Nitric 2”, or leave the method to the processor.
  • ASTM A380 is a broader practice for cleaning, descaling and passivating stainless parts and systems; it gives guidance rather than acceptance criteria.
  • AMS 2700 is the aerospace counterpart, also covering nitric and citric methods.
  • 303 needs care: strong nitric treatments can attack the sulfide inclusions and cause surface etching or "flash" attack. Tell the processor the grade so they choose a suitable method.

What to write on the drawing

A grade name alone leaves the supplier to choose standard and condition. A complete material note looks like “Stainless steel 316L (1.4404), annealed, passivate per ASTM A967”. Checklist:

  • Grade with EN or UNS number (S30300, S30400, S31600/S31603) so a European or Asian mill equivalent is unambiguous.
  • Whether substitution is allowed: “303 acceptable” on a 304 callout can lower cost if corrosion and welding allow.
  • Condition, normally annealed (solution treated); state it if you need cold-drawn bar for strength.
  • Passivation requirement and standard, and whether a test report is needed.
  • Mill inspection document (EN 10204 type 3.1 is the common request) if traceability matters.
  • Surface finish (Ra) on functional surfaces, and any requirement for bead blasting or electropolishing.

Stainless steel parts at Chi Xin

Chi Xin Technology is a CNC machine shop in Nantun District, Taichung, Taiwan, founded in 2022. We run 5+ CNC machines — 4.5-axis CNC machining centers and CNC lathes — and mainly machine aluminum alloys and alloy steel, with a metal tolerance of 0.02 mm. We also offer wire EDM and surface finishing including anodizing, and we export to customers in Europe and North America.

Stainless steel parts are part of our catalog alongside aluminum and alloy steel, made on the same CNC lathes and 4.5-axis machining centers; if you need passivation, a specific bar standard or a mill inspection document, tell us in the RFQ and we confirm in the quotation.

Frequently asked questions

Can I substitute 303 for 304 to reduce cost?

Often yes for parts that are not welded and not exposed to chlorides or acids. Check the environment first; if in doubt, keep 304 or ask the supplier to quote both grades.

Is 316 always better than 304?

For corrosion in chloride environments, yes. For indoor or dry use the difference rarely matters, and 316 costs more as raw material, so 304 is usually the sensible default.

Do I need 316L or is 316 enough?

For parts that are welded or used after welding without re-annealing, specify 316L to reduce sensitization. For machined parts that are never welded, 316 and 316L behave much the same, and dual-grade bar covers both.

Why are my 304 parts slightly magnetic?

Cold work from drawing the bar and from machining can transform some austenite to martensite near the surface. It does not mean the wrong grade was used, but if non-magnetic behaviour matters, state a permeability limit on the drawing.

Is passivation required after machining?

It is not mandatory, but it is good practice for parts in corrosive service or with hygiene requirements. Specify it on the drawing with ASTM A967 or AMS 2700 so it is quoted and done consistently.

Parts we have machined

Browse custom parts →
CNC machined stainless steel valve body
Valve Bodystainless steel
CNC machined steel connector
Connectorsteel
CNC machined stainless steel sleeve
Sleevestainless steel
CNC machined steel flange valve body
Flange Valve Bodysteel

Have a drawing ready?

Upload your drawing or CAD file and get a quote.

Get a Quote
WhatsAppEmail drawings