CNC Turning for PEEK (Polyether Ether Ketone)
Turning PEEK requires managing heat to prevent changes in crystallinity and dimensional instability. Sharp tooling and appropriate speeds produce excellent results.
Parametres d'usinage recommandes
| Parametre | Valeur |
|---|---|
| Tolerances realisables | ±0.02 mm (±0.001") |
| Etat de surface | Ra 0.8-3.2 μm |
| Vitesse de coupe | 150-300 m/min |
| Vitesse d'avance | 0.05-0.15 mm/rev |
| Outillage recommande | Sharp uncoated carbide or PCD. Positive rake angle. Polished insert face to reduce friction. |
Conseils d'usinage expert
1
Use compressed air cooling — avoid oil contamination
2
Sharp positive inserts essential
3
Light finishing cuts for best tolerance
4
Support long parts to prevent deflection
Pieces couramment fabriquees
Bearing sleeves
Seal rings
Surgical instrument handles
Electrical insulator bushings
Valve seats
Defis d'usinage
- High material cost — minimize scrap
- Thermal expansion during machining
- Difficult to hold concentricity on long parts