CNC Milling for PEEK (Polyether Ether Ketone)
CNC milling PEEK requires understanding its unique properties as a semi-crystalline thermoplastic. Proper thermal management is critical — too much heat changes crystallinity and dimensions.
建議加工參數
| 參數 | 數值 |
|---|---|
| 可達公差 | ±0.02 mm (±0.001") |
| 表面光潔度 | Ra 0.8-3.2 μm |
| 切削速度 | 100-250 m/min (SFM 330-820) |
| 進給速率 | 0.05-0.15 mm/tooth |
| 刀具建議 | Sharp uncoated carbide, 2-3 flutes with polished flutes. O-flute single-flute for finishing. |
專家加工技巧
1
Use sharp, uncoated carbide tools
2
Moderate speeds to avoid melting
3
Compressed air cooling preferred (no oil contamination)
4
Support thin walls to prevent deflection
5
Anneal stock before machining for stability
常見加工零件
Semiconductor fixtures
Medical device housings
Bearing retainers
Valve seats
Electrical insulators
加工挑戰
- Material cost ($100+/kg) — minimize scrap
- Thermal expansion during machining
- Crystallinity changes affect properties
- Dust can irritate lungs (use extraction)