Surface Finishing for Aluminum 7075-T6
7075 aluminum anodizes differently than 6061 — it tends toward yellow/brown hues and does not color as vibrantly. Chromate conversion and hardcoat are more common finishes.
권장 가공 매개변수
| 매개변수 | 값 |
|---|---|
| 달성 가능 공차 | ±0.02 mm (±0.0008") |
| 표면 조도 | Ra 0.4-3.2 μm |
| 절삭 속도 | N/A |
| 이송 속도 | N/A |
| 공구 추천 | N/A — surface finishing process |
전문가 가공 팁
1
Expect darker/yellower anodize than 6061
2
Hardcoat (Type III) works well
3
Chromate conversion preferred for aerospace
4
Clear anodize may have a slight yellow tint
일반 가공 부품
Chromated aerospace parts
Hardcoated wear surfaces
Clear anodized defense components
가공 과제
- Anodize color less vibrant than 6061
- Zinc content affects color consistency
- Not ideal for colored decorative anodize