Surface Finishing for Aluminum 7075-T6
7075 aluminum anodizes differently than 6061 — it tends toward yellow/brown hues and does not color as vibrantly. Chromate conversion and hardcoat are more common finishes.
Parametres d'usinage recommandes
| Parametre | Valeur |
|---|---|
| Tolerances realisables | ±0.02 mm (±0.0008") |
| Etat de surface | Ra 0.4-3.2 μm |
| Vitesse de coupe | N/A |
| Vitesse d'avance | N/A |
| Outillage recommande | N/A — surface finishing process |
Conseils d'usinage expert
1
Expect darker/yellower anodize than 6061
2
Hardcoat (Type III) works well
3
Chromate conversion preferred for aerospace
4
Clear anodize may have a slight yellow tint
Pieces couramment fabriquees
Chromated aerospace parts
Hardcoated wear surfaces
Clear anodized defense components
Defis d'usinage
- Anodize color less vibrant than 6061
- Zinc content affects color consistency
- Not ideal for colored decorative anodize