Surface Finishing for Titanium Grade 5 (Ti-6Al-4V)
Titanium naturally forms a protective oxide layer, but surface treatments can enhance performance. Anodizing provides colors, PVD adds wear resistance, and shot peening improves fatigue life.
Parametros de mecanizado recomendados
| Parametro | Valor |
|---|---|
| Tolerancias alcanzables | ±0.02 mm (±0.0008") |
| Acabado superficial | Ra 0.4-3.2 μm |
| Velocidad de corte | N/A |
| Velocidad de avance | N/A |
| Herramientas recomendadas | N/A — surface finishing process |
Consejos de mecanizado experto
1
Type II anodize for colored identification coding
2
PVD (TiN, TiAlN) for wear resistance
3
Shot peen for fatigue life improvement (compressive stress)
4
Passivation removes free iron contamination
Piezas comunes fabricadas
Anodized aerospace fasteners
PVD-coated surgical instruments
Shot-peened structural parts
Desafios de mecanizado
- Titanium anodize is different from aluminum anodize
- PVD coating temperature must not degrade Ti properties
- Color anodize for identification, not protection
Otros materiales para Surface Finishing
Otros procesos para Titanium Grade 5 (Ti-6Al-4V)
Listo para comenzar el mecanizado?
Suba su plano o archivo CAD y reciba una cotización.
Solicitar presupuesto gratuito