CNC Milling for Delrin (POM / Acetal)

Delrin is one of the best plastics for CNC milling, producing clean chips and excellent surface finishes. Its high stiffness allows tight tolerances to be held reliably.

Parametros de mecanizado recomendados

ParametroValor
Tolerancias alcanzables±0.02 mm (±0.001")
Acabado superficialRa 0.4-1.6 μm
Velocidad de corte150-400 m/min (SFM 500-1300)
Velocidad de avance0.08-0.20 mm/tooth
Herramientas recomendadasSharp uncoated carbide, 2 flutes with high helix for chip evacuation. O-flute end mills for fine finish.

Consejos de mecanizado experto

1

High speeds and feeds for clean chip formation

2

Use sharp tools to prevent melting

3

Air cooling is usually sufficient

4

Avoid heavy depths of cut on thin walls

5

Allow material to stabilize at room temp before final cuts

Piezas comunes fabricadas

Gears and sprockets

Bearing bushings

Conveyor guides

Pump impellers

Precision spacers

Desafios de mecanizado

  • Chips can melt and re-weld if speed too high
  • Material expands with temperature
  • Cannot be painted or glued easily

Listo para comenzar el mecanizado?