Nylon 6 vs Nylon 66 for CNC Machining: Key Differences

Nylon 6 is more cost-effective with better impact resistance and easier processing. Nylon 66 offers higher heat resistance and stiffness, making it better for automotive under-hood and electrical applications.

並列特性比較

特性Nylon 6 (PA6)Nylon 66 (PA66)
抗拉強度79 MPa (11.5 ksi)82 MPa (11.9 ksi)
屈服強度70 MPa (10.2 ksi)69 MPa (10 ksi)
硬度Rockwell R119Rockwell R120
密度1.14 g/cm³1.14 g/cm³
可加工性評級70/10068/100
熱傳導率0.25 W/m·K0.26 W/m·K
熔點220 °C262 °C
公差±0.05 mm±0.05 mm

主要差異

特性Nylon 6 (PA6)Nylon 66 (PA66)優勝
Melting Point220°C262°CNylon
StiffnessGoodBetterNylon
Impact ResistanceExcellentGoodNylon
CostLowerHigherNylon
Moisture Absorption9.5% (saturated)8.5% (saturated)Nylon
Machinability70/10068/100Nylon

您應該選擇哪種材料?

選擇 Nylon 6 (PA6) 當:

  • General-purpose mechanical parts
  • Impact-loaded components
  • Budget-sensitive projects
  • Cast nylon for large parts
  • Wear pads and rollers
查看詳情 Nylon 6 (PA6)→

選擇 Nylon 66 (PA66) 當:

  • Automotive under-hood components
  • Electrical housings
  • Higher temperature applications
  • Parts needing better rigidity
  • Glass-filled structural components
查看詳情 Nylon 66 (PA66)→

不確定選擇哪種材料?

我們的工程師可以為您的應用推薦最佳材料。上傳設計圖獲取免費諮詢。