Nylon vs Delrin (POM) for CNC Parts: Which Plastic to Choose?

Delrin excels in dimensional stability and low friction for precision parts like gears and bearings. Nylon offers better impact resistance and higher temperature performance but absorbs more moisture, causing dimensional changes.

특성 비교

특성Nylon 66 (PA66)Delrin (POM / Acetal)
인장강도82 MPa (11.9 ksi)70 MPa (10.2 ksi)
항복강도69 MPa (10 ksi)65 MPa (9.4 ksi)
경도Rockwell R120Rockwell M80
밀도1.14 g/cm³1.42 g/cm³
절삭성 등급68/10085/100
열전도율0.26 W/m·K0.31 W/m·K
용융점262 °C175 °C
공차±0.05 mm±0.02 mm

주요 차이점

특성Nylon 66 (PA66)Delrin (POM / Acetal)우수
Dimensional StabilityFair (moisture)ExcellentDelrin
Moisture Absorption2.5%0.25%Delrin
Impact ResistanceExcellentGoodNylon
Friction Coefficient0.30-0.400.20-0.35Delrin
Temperature RangeUp to 120°CUp to 100°CNylon
Machinability68/10085/100Delrin

어떤 소재를 선택해야 할까요?

선택 Nylon 66 (PA66) 할 때:

  • Impact-loaded components
  • Higher temperature applications (up to 120°C)
  • Parts needing better chemical resistance
  • Under-hood automotive components
  • Structural parts requiring toughness
상세 보기 Nylon 66 (PA66)→

선택 Delrin (POM / Acetal) 할 때:

  • Precision gears and bearings
  • Parts with tight tolerances
  • Low-friction sliding surfaces
  • Humid or wet environments
  • Food processing equipment
상세 보기 Delrin (POM / Acetal)→

어떤 소재를 선택할지 모르시겠나요?

엔지니어가 귀하의 용도에 최적인 소재를 추천해 드립니다. 무료 상담을 위해 설계도를 업로드하세요.