Nylon vs Delrin (POM) for CNC Parts: Which Plastic to Choose?
Delrin excels in dimensional stability and low friction for precision parts like gears and bearings. Nylon offers better impact resistance and higher temperature performance but absorbs more moisture, causing dimensional changes.
特性の並列比較
| 特性 | Nylon 66 (PA66) | Delrin (POM / Acetal) |
|---|---|---|
| 引張強度 | 82 MPa (11.9 ksi) | 70 MPa (10.2 ksi) |
| 降伏強度 | 69 MPa (10 ksi) | 65 MPa (9.4 ksi) |
| 硬度 | Rockwell R120 | Rockwell M80 |
| 密度 | 1.14 g/cm³ | 1.42 g/cm³ |
| 被削性評価 | 68/100 | 85/100 |
| 熱伝導率 | 0.26 W/m·K | 0.31 W/m·K |
| 融点 | 262 °C | 175 °C |
| 公差 | ±0.05 mm | ±0.02 mm |
主な違い
| 特性 | Nylon 66 (PA66) | Delrin (POM / Acetal) | 優位 |
|---|---|---|---|
| Dimensional Stability | Fair (moisture) | Excellent | Delrin |
| Moisture Absorption | 2.5% | 0.25% | Delrin |
| Impact Resistance | Excellent | Good | Nylon |
| Friction Coefficient | 0.30-0.40 | 0.20-0.35 | Delrin |
| Temperature Range | Up to 120°C | Up to 100°C | Nylon |
| Machinability | 68/100 | 85/100 | Delrin |
どちらの素材を選ぶべきですか?
選択 Nylon 66 (PA66) の場合:
- Impact-loaded components
- Higher temperature applications (up to 120°C)
- Parts needing better chemical resistance
- Under-hood automotive components
- Structural parts requiring toughness
選択 Delrin (POM / Acetal) の場合:
- Precision gears and bearings
- Parts with tight tolerances
- Low-friction sliding surfaces
- Humid or wet environments
- Food processing equipment