Aluminum 7075 vs Titanium Grade 5: Aerospace Material Showdown

Aluminum 7075 is significantly cheaper and easier to machine, making it the default for non-critical aerospace structures. Titanium Grade 5 wins when maximum strength-to-weight, temperature resistance, or corrosion resistance is non-negotiable.

特性の並列比較

特性Aluminum 7075-T6Titanium Grade 5 (Ti-6Al-4V)
引張強度572 MPa (83 ksi)950 MPa (138 ksi)
降伏強度503 MPa (73 ksi)880 MPa (128 ksi)
硬度150 HB334 HV
密度2.81 g/cm³4.43 g/cm³
被削性評価70/10022/100
熱伝導率130 W/m·K6.7 W/m·K
融点477–635 °C1,604–1,660 °C
公差±0.02 mm±0.02 mm

主な違い

特性Aluminum 7075-T6Titanium Grade 5 (Ti-6Al-4V)優位
Strength-to-Weight203 kNm/kg214 kNm/kgTitanium
Machinability70/10022/100Aluminum
Cost per Part1x (baseline)5-10xAluminum
Corrosion ResistanceGoodExcellentTitanium
Max Service Temp120°C315°CTitanium
Density2.81 g/cm³4.43 g/cm³Aluminum

どちらの素材を選ぶべきですか?

選択 Aluminum 7075-T6 の場合:

  • Cost-sensitive aerospace parts
  • High-volume production
  • Room-temperature applications
  • Non-critical structural components
  • Where machinability matters
詳細を見る Aluminum 7075-T6→

選択 Titanium Grade 5 (Ti-6Al-4V) の場合:

  • Elevated temperature (>150°C) components
  • Maximum strength-to-weight ratio
  • Corrosive environments
  • Biomedical implants
  • Engine and turbine components
詳細を見る Titanium Grade 5 (Ti-6Al-4V)→

どの素材を選べばよいかわかりませんか?

当社のエンジニアがお客様の用途に最適な素材を推奨します。無料相談のためにデザインをアップロードしてください。

無料見積もりを取得