Nylon vs Delrin (POM) for CNC Parts: Which Plastic to Choose?
Delrin excels in dimensional stability and low friction for precision parts like gears and bearings. Nylon offers better impact resistance and higher temperature performance but absorbs more moisture, causing dimensional changes.
Comparaison des proprietes
| Propriete | Nylon 66 (PA66) | Delrin (POM / Acetal) |
|---|---|---|
| Resistance a la traction | 82 MPa (11.9 ksi) | 70 MPa (10.2 ksi) |
| Limite elastique | 69 MPa (10 ksi) | 65 MPa (9.4 ksi) |
| Durete | Rockwell R120 | Rockwell M80 |
| Densite | 1.14 g/cm³ | 1.42 g/cm³ |
| Indice d'usinabilite | 68/100 | 85/100 |
| Conductivite thermique | 0.26 W/m·K | 0.31 W/m·K |
| Point de fusion | 262 °C | 175 °C |
| Tolerance | ±0.05 mm | ±0.02 mm |
Differences cles
| Propriete | Nylon 66 (PA66) | Delrin (POM / Acetal) | Gagnant |
|---|---|---|---|
| Dimensional Stability | Fair (moisture) | Excellent | Delrin |
| Moisture Absorption | 2.5% | 0.25% | Delrin |
| Impact Resistance | Excellent | Good | Nylon |
| Friction Coefficient | 0.30-0.40 | 0.20-0.35 | Delrin |
| Temperature Range | Up to 120°C | Up to 100°C | Nylon |
| Machinability | 68/100 | 85/100 | Delrin |
Quel materiau choisir ?
Choisissez Nylon 66 (PA66) quand:
- Impact-loaded components
- Higher temperature applications (up to 120°C)
- Parts needing better chemical resistance
- Under-hood automotive components
- Structural parts requiring toughness
Choisissez Delrin (POM / Acetal) quand:
- Precision gears and bearings
- Parts with tight tolerances
- Low-friction sliding surfaces
- Humid or wet environments
- Food processing equipment
Pas sur du materiau a choisir ?
Nos ingenieurs peuvent recommander le meilleur materiau pour votre application. Telechargez votre conception pour une consultation gratuite.