Aluminum 5052 vs 6061: Sheet Metal vs Structural CNC
5052 excels in saltwater corrosion resistance and formability for sheet metal applications. 6061 provides significantly higher strength and better machinability for structural CNC machined components.
Comparaison des proprietes
| Propriete | Aluminum 5052-H32 | Aluminum 6061-T6 |
|---|---|---|
| Resistance a la traction | 228 MPa (33 ksi) | 310 MPa (45 ksi) |
| Limite elastique | 193 MPa (28 ksi) | 276 MPa (40 ksi) |
| Durete | 60 HB | 95 HB (Brinell) |
| Densite | 2.68 g/cm³ | 2.70 g/cm³ |
| Indice d'usinabilite | 60/100 | 90/100 |
| Conductivite thermique | 138 W/m·K | 167 W/m·K |
| Point de fusion | 607–649 °C | 582–652 °C |
| Tolerance | ±0.02 mm | ±0.02 mm |
Differences cles
| Propriete | Aluminum 5052-H32 | Aluminum 6061-T6 | Gagnant |
|---|---|---|---|
| Tensile Strength | 228 MPa | 310 MPa | Aluminum |
| Machinability | 60/100 | 90/100 | Aluminum |
| Saltwater Resistance | Excellent | Good | Aluminum |
| Formability | Excellent | Good | Aluminum |
| Heat Treatable | No | Yes (T6) | Aluminum |
| Cost | Similar | Similar | Egalite |
Quel materiau choisir ?
Choisissez Aluminum 5052-H32 quand:
- Marine and saltwater applications
- Sheet metal formed parts
- Fuel tanks and pressure vessels
- Electronic chassis and enclosures
- Parts requiring deep drawing
Choisissez Aluminum 6061-T6 quand:
- Structural components
- CNC machined parts (better machinability)
- Heat-treatable applications
- Parts requiring higher strength
- General-purpose machined parts
Pas sur du materiau a choisir ?
Nos ingenieurs peuvent recommander le meilleur materiau pour votre application. Telechargez votre conception pour une consultation gratuite.
Devis gratuit