Turning PEEK requires managing heat to prevent changes in crystallinity and dimensional instability. Sharp tooling and appropriate speeds produce excellent results.

Parametros de mecanizado recomendados

ParametroValor
Tolerancias alcanzables±0.02 mm (±0.001")
Acabado superficialRa 0.8-3.2 μm
Velocidad de corte150-300 m/min
Velocidad de avance0.05-0.15 mm/rev
Herramientas recomendadasSharp uncoated carbide or PCD. Positive rake angle. Polished insert face to reduce friction.

Consejos de mecanizado experto

1

Use compressed air cooling — avoid oil contamination

2

Sharp positive inserts essential

3

Light finishing cuts for best tolerance

4

Support long parts to prevent deflection

Piezas comunes fabricadas

Bearing sleeves

Seal rings

Surgical instrument handles

Electrical insulator bushings

Valve seats

Desafios de mecanizado

  • High material cost — minimize scrap
  • Thermal expansion during machining
  • Difficult to hold concentricity on long parts