Nylon 6 vs Nylon 66 for CNC Machining: Key Differences
Nylon 6 is more cost-effective with better impact resistance and easier processing. Nylon 66 offers higher heat resistance and stiffness, making it better for automotive under-hood and electrical applications.
Comparacion de propiedades
| Propiedad | Nylon 6 (PA6) | Nylon 66 (PA66) |
|---|---|---|
| Resistencia a la traccion | 79 MPa (11.5 ksi) | 82 MPa (11.9 ksi) |
| Limite elastico | 70 MPa (10.2 ksi) | 69 MPa (10 ksi) |
| Dureza | Rockwell R119 | Rockwell R120 |
| Densidad | 1.14 g/cm³ | 1.14 g/cm³ |
| Indice de maquinabilidad | 70/100 | 68/100 |
| Conductividad termica | 0.25 W/m·K | 0.26 W/m·K |
| Punto de fusion | 220 °C | 262 °C |
| Tolerancia | ±0.05 mm | ±0.05 mm |
Diferencias clave
| Propiedad | Nylon 6 (PA6) | Nylon 66 (PA66) | Ganador |
|---|---|---|---|
| Melting Point | 220°C | 262°C | Nylon |
| Stiffness | Good | Better | Nylon |
| Impact Resistance | Excellent | Good | Nylon |
| Cost | Lower | Higher | Nylon |
| Moisture Absorption | 9.5% (saturated) | 8.5% (saturated) | Nylon |
| Machinability | 70/100 | 68/100 | Nylon |
Que material deberia elegir?
Elija Nylon 6 (PA6) cuando:
- General-purpose mechanical parts
- Impact-loaded components
- Budget-sensitive projects
- Cast nylon for large parts
- Wear pads and rollers
Elija Nylon 66 (PA66) cuando:
- Automotive under-hood components
- Electrical housings
- Higher temperature applications
- Parts needing better rigidity
- Glass-filled structural components