Comparacion de propiedades

PropiedadAluminum 7075-T6Titanium Grade 5 (Ti-6Al-4V)
Resistencia a la traccion572 MPa (83 ksi)950 MPa (138 ksi)
Limite elastico503 MPa (73 ksi)880 MPa (128 ksi)
Dureza150 HB334 HV
Densidad2.81 g/cm³4.43 g/cm³
Indice de maquinabilidad70/10022/100
Conductividad termica130 W/m·K6.7 W/m·K
Punto de fusion477–635 °C1,604–1,660 °C
Tolerancia±0.02 mm±0.02 mm

Diferencias clave

PropiedadAluminum 7075-T6Titanium Grade 5 (Ti-6Al-4V)Ganador
Strength-to-Weight203 kNm/kg214 kNm/kgTitanium
Machinability70/10022/100Aluminum
Cost per Part1x (baseline)5-10xAluminum
Corrosion ResistanceGoodExcellentTitanium
Max Service Temp120°C315°CTitanium
Density2.81 g/cm³4.43 g/cm³Aluminum

Que material deberia elegir?

Elija Aluminum 7075-T6 cuando:

  • Cost-sensitive aerospace parts
  • High-volume production
  • Room-temperature applications
  • Non-critical structural components
  • Where machinability matters
Ver detalles Aluminum 7075-T6→

Elija Titanium Grade 5 (Ti-6Al-4V) cuando:

  • Elevated temperature (>150°C) components
  • Maximum strength-to-weight ratio
  • Corrosive environments
  • Biomedical implants
  • Engine and turbine components
Ver detalles Titanium Grade 5 (Ti-6Al-4V)→

No esta seguro de que material elegir?

Nuestros ingenieros pueden recomendar el mejor material para su aplicacion. Suba su diseno para una consulta gratuita.

Solicitar presupuesto gratuito