Aluminum 7075 vs Titanium Grade 5: Aerospace Material Showdown

Aluminum 7075 is significantly cheaper and easier to machine, making it the default for non-critical aerospace structures. Titanium Grade 5 wins when maximum strength-to-weight, temperature resistance, or corrosion resistance is non-negotiable.

Eigenschaftsvergleich

EigenschaftAluminum 7075-T6Titanium Grade 5 (Ti-6Al-4V)
Zugfestigkeit572 MPa (83 ksi)950 MPa (138 ksi)
Streckgrenze503 MPa (73 ksi)880 MPa (128 ksi)
Haerte150 HB334 HV
Dichte2.81 g/cm³4.43 g/cm³
Zerspanbarkeit70/10022/100
Waermeleitfaehigkeit130 W/m·K6.7 W/m·K
Schmelzpunkt477–635 °C1,604–1,660 °C
Toleranz±0.02 mm±0.02 mm

Hauptunterschiede

EigenschaftAluminum 7075-T6Titanium Grade 5 (Ti-6Al-4V)Gewinner
Strength-to-Weight203 kNm/kg214 kNm/kgTitanium
Machinability70/10022/100Aluminum
Cost per Part1x (baseline)5-10xAluminum
Corrosion ResistanceGoodExcellentTitanium
Max Service Temp120°C315°CTitanium
Density2.81 g/cm³4.43 g/cm³Aluminum

Welches Material sollten Sie waehlen?

Waehlen Sie Aluminum 7075-T6 wenn:

  • Cost-sensitive aerospace parts
  • High-volume production
  • Room-temperature applications
  • Non-critical structural components
  • Where machinability matters
Details anzeigen Aluminum 7075-T6→

Waehlen Sie Titanium Grade 5 (Ti-6Al-4V) wenn:

  • Elevated temperature (>150°C) components
  • Maximum strength-to-weight ratio
  • Corrosive environments
  • Biomedical implants
  • Engine and turbine components
Details anzeigen Titanium Grade 5 (Ti-6Al-4V)→

Unsicher welches Material?

Unsere Ingenieure empfehlen das beste Material fuer Ihre Anwendung. Laden Sie Ihr Design fuer eine kostenlose Beratung hoch.

Kostenloses Angebot