Aluminum 6061 vs Brass C360 for CNC: Lightweight vs Machinability

Aluminum 6061 wins on weight (3x lighter) and overall versatility. Brass C360 wins on pure machinability and is preferred for fittings, connectors, and decorative parts where its gold appearance and conductivity are advantages.

Eigenschaftsvergleich

EigenschaftAluminum 6061-T6Brass C360 (Free-Cutting Brass)
Zugfestigkeit310 MPa (45 ksi)385 MPa (56 ksi)
Streckgrenze276 MPa (40 ksi)310 MPa (45 ksi)
Haerte95 HB (Brinell)78 HRB
Dichte2.70 g/cm³8.49 g/cm³
Zerspanbarkeit90/100100/100
Waermeleitfaehigkeit167 W/m·K115 W/m·K
Schmelzpunkt582–652 °C885–900 °C
Toleranz±0.02 mm±0.02 mm

Hauptunterschiede

EigenschaftAluminum 6061-T6Brass C360 (Free-Cutting Brass)Gewinner
Weight (Density)2.70 g/cm³8.49 g/cm³Aluminum
Machinability90/100100/100Brass
Tensile Strength310 MPa385 MPaBrass
Thermal Conductivity167 W/m·K115 W/m·KAluminum
Cost per kg~$6~$7Aluminum
Corrosion ResistanceExcellentGoodAluminum

Welches Material sollten Sie waehlen?

Waehlen Sie Aluminum 6061-T6 wenn:

  • Weight-critical applications
  • Structural components
  • Heat sinks (better thermal performance)
  • Large parts where weight adds up
  • Anodized finish desired
Details anzeigen Aluminum 6061-T6→

Waehlen Sie Brass C360 (Free-Cutting Brass) wenn:

  • Fittings and connectors
  • High-volume screw machine parts
  • Decorative or luxury hardware
  • Electrical terminals
  • Plumbing components
Details anzeigen Brass C360 (Free-Cutting Brass)→

Unsicher welches Material?

Unsere Ingenieure empfehlen das beste Material fuer Ihre Anwendung. Laden Sie Ihr Design fuer eine kostenlose Beratung hoch.

Kostenloses Angebot